Mineralogical composition:
Al2O3 content 27 %
Bulk density 2.42 g/cm3
Apparent density 19.0 %
Water absorption 7.8 %
M.O.E. 20°C > 90 GPa
Thermal expansion at 400°C 5.5 (K-1 10-6)
Application:
Notes: recommended in rapid cooling zones for an aligned advancement of the tiles.